Between 230 and 370°C, blue brittleness is caused in mild steel because of the

Question: Between 230 and 370°C, blue brittleness is caused in mild steel because of the
[A].

immobility of dislocation.

[B].

strain-ageing.

[C].

increase in Young’s modulus.

[D].

strain hardening.

Answer: Option B

Explanation: