A form of stress corrosion failure termed as ‘season cracking’ is generally observed in

Question: A form of stress corrosion failure termed as ‘season cracking’ is generally observed in
[A].

thermosetting polymers.

[B].

high carbon steels.

[C].

brasses.

[D].

borosilicate glasses.

Answer: Option C

Explanation:

No answer description available for this question.