Question: Cold cracking in the heat affected zone of a high strength steel weld can take place because of the
[A]. retained austenite.
relatively high sulphur content in the base metal.
[A]. retained austenite.
[B].
martensite formation.[C].
[D].
sufficient hydrogen present in the welding arc.Answer: Option B
Explanation:
No answer description available for this question.