In spheroidising process, the steel is

Question: In spheroidising process, the steel is
[A].

heated below the lower critical temperature and then cooled slowly

[B].

heated upto the lower critical temperature and then cooled in still air

[C].

heated slightly above the lower critical temperature and then cooled slowly to a temperature of 600°C

[D].

none of the above

Answer: Option C

Explanation:

No answer description available for this question.

In process annealing, the hypo-eutectoid steel is

Question: In process annealing, the hypo-eutectoid steel is
[A].

heated from 30° C to 50° C above the upper critical temperature and then cooled in still air

[B].

heated from 30° C to 50° C above the upper critical temperature and then cooled suddenly in a suitable cooling medium

[C].

heated from 30° C to 50° C above the upper critical temperature and then cooled slowly in the furnace

[D].

heated below or close to the lower critical temperature and then cooled slowly

Answer: Option D

Explanation:

No answer description available for this question.

In full annealing, the hypo-eutectoid steel is heated from 30° C to 50° C above the upper critical temperature and then cooled

Question: In full annealing, the hypo-eutectoid steel is heated from 30° C to 50° C above the upper critical temperature and then cooled
[A].

in still air

[B].

slowly in the furnace

[C].

suddenly in a suitable cooling medium

[D].

any one of these

Answer: Option B

Explanation:

No answer description available for this question.

In normalising process, the hypo-eutectiod steel is heated from 30° C to 50° C above the upper critical temperature and then cooled in still air.

Question: In normalising process, the hypo-eutectiod steel is heated from 30° C to 50° C above the upper critical temperature and then cooled in still air.
[A].

True

[B].

False

Answer: Option A